OK Autrod 12.24

ESAB

OK Autrod 12.24

The following items have been added to your list


x

OK Autrod 12.24 is a copper-coated, molybdenum-alloyed wire for the submerged arc welding of non-alloyed and low-alloyed steels. It can be combined with OK Flux 10.47, OK Flux 10.61, OK Flux 10.62, OK Flux 10.71, OK Flux 10.72, OK Flux 10.73, OK Flux 10.81 and OK Flux 10.83.

BUY NOW


Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Mn Mo Ni P S Si
0.10 % 0.04 % 1.06 % 0.50 % 0.02 % 0.013 % 0.014 % 0.15 %

Approvals

Approvals CE EN 13479
CZ : NAKS/HAKC 2.0-5.0 mm
Approvals are based on factory location. Please contact ESAB for more information.

Classifications

Name SFA/AWS A5.23
Grade EA2
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod 12.24
OK Autrod 12.24 1.6mm 15kg 1224167600 FIND A DISTRIBUTOR
OK Autrod 12.24 1.6mm 475kg 1224169400 FIND A DISTRIBUTOR
OK Autrod 12.24 2.0mm 100kg 1224205200 FIND A DISTRIBUTOR
OK Autrod 12.24 2.0mm 30kg 1224202800 FIND A DISTRIBUTOR
OK Autrod 12.24 2.0mm 450kg 1224209420 FIND A DISTRIBUTOR
OK Autrod 12.24 2.5mm 1000kg 1224253330 FIND A DISTRIBUTOR
OK Autrod 12.24 2.5mm 25kg 1224252810 FIND A DISTRIBUTOR
OK Autrod 12.24 2.5mm 280kg 122425040F FIND A DISTRIBUTOR
OK Autrod 12.24 2.5mm 300kg 1224253400 FIND A DISTRIBUTOR
OK Autrod 12.24 2.5mm 30kg 1224252800 FIND A DISTRIBUTOR
OK Autrod 12.24 3.0mm 1000kg 1224303330 FIND A DISTRIBUTOR
OK Autrod 12.24 3.0mm 25kg 1224302810 FIND A DISTRIBUTOR
OK Autrod 12.24 3.0mm 30kg 1224302800 FIND A DISTRIBUTOR
OK Autrod 12.24 3.2mm 1000kg 1224323330 FIND A DISTRIBUTOR
OK Autrod 12.24 3.2mm 1000kg 122432333F FIND A DISTRIBUTOR
OK Autrod 12.24 3.2mm 100kg 1224325200 FIND A DISTRIBUTOR
OK Autrod 12.24 3.2mm 100kg 122432520F FIND A DISTRIBUTOR
OK Autrod 12.24 3.2mm 30kg 1224322800 FIND A DISTRIBUTOR
OK Autrod 12.24 3.2mm 350kg 1224320600 FIND A DISTRIBUTOR
OK Autrod 12.24 3/16 800lb 122448132N FIND A DISTRIBUTOR
OK AUTROD 12.24 3/32X65#CL 122424120N FIND A DISTRIBUTOR
OK Autrod 12.24 4.0mm 1000kg 1224403330 FIND A DISTRIBUTOR
OK Autrod 12.24 4.0mm 1000kg 122440333F FIND A DISTRIBUTOR
OK Autrod 12.24 4.0mm 100kg 1224405200 FIND A DISTRIBUTOR
OK Autrod 12.24 4.0mm 100kg 122440520F FIND A DISTRIBUTOR
OK Autrod 12.24 4.0mm 25kg 1224402810 FIND A DISTRIBUTOR
OK Autrod 12.24 4.0mm 30kg 1224402800 FIND A DISTRIBUTOR
OK Autrod 12.24 4.0mm 350kg 1224400600 FIND A DISTRIBUTOR
OK Autrod 12.24 4.0mm 800kg 1224401841 FIND A DISTRIBUTOR
OK AUTROD 12.24 5.0MM 100KG 1224505200 FIND A DISTRIBUTOR
OK AUTROD 12.24 5.0MM 30K 1224502800 FIND A DISTRIBUTOR
OK AUTROD 12.24 5/32X65#CL 122440120N FIND A DISTRIBUTOR
x
x

x

Loading..