Alloy Shield 70S
Alloy Shield 70S is a metal-cored wire used for submerged arc welding applications. It is designed for similar applications as solid wire classification EM12K, including structural steel, shipbuilding, tank fabrication, wheel fabrication, heavy equipment, offshore fabrication, and transmission poles. It can be used to weld over light mill scale and rust while still producing quality welds.
Industries
- Ship and Offshore Yards
- Ship/Barge Building
- Tank and Vessel Fabrication
- Heavy Equipment
- Structural Steel Fabrication
Welding Process
- SAW - Submerged Arc Welding
Classifications
Grade | EC1 |
Name | AWS A5.17 |
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Mn | P | S | Si | ||||||||||
0.086 % | 1.43 % | 0.014 % | 0.014 % | 0.49 % |
*With OK Flux 10.71 | Typical Weld Metal Analysis with OK Flux 10.71