ThermaClad 42 is a new improved alloy designed for build up and overlay of undercarriage components. The alloy composition gives an optimum combination of strength, toughness.

BUY NOW


Features

  • Temper resistance and insensitivity to cooling rate.
  • It also resists metal-to-metal frictional wear.
  • Deposit hardness is approximately 40 - 42 HRC in two layers.


Specifications


Typical Weld Metal Analysis

OtherCCrFe
4.0 %0.2 %2.9 %BAL %

x

Typical Weld Metal Analysis

OtherCCrFe
4.0 %0.2 %2.9 %BAL %