ThermaClad 105B deposit has very good resistance to metal-to-metal-wear. The deposits are readily machinable with carbide tools. Multiple layer, crack-free deposits can be obtained. When more than four layers are required, an underbase of ThermaClad 104 is recommended. Deposits are difficult to flame cut.

BUY NOW


Specifications


Typical Tensile Properties

Hardness (HRC)
42 HRC

Typical Weld Metal Analysis

OtherCCrFe
4.5 %0.5 %3.5 %BAL %

x

Typical Tensile Properties

Hardness (HRC)
42 HRC

Typical Weld Metal Analysis

OtherCCrFe
4.5 %0.5 %3.5 %BAL %