ThermaClad 104 deposit has excellent resistance to impact and plastic deformation. Deposits are machinable with high speed tools, easily machinable with carbide tools, crack-free, and can be flame cut. ThermaClad 104 is ideal for build-up and for underbase to support hardfacing. Maximum deposit thickness is unlimited.

BUY NOW


Specifications


Typical Tensile Properties

Elongation Hardness (HRC) Tensile Strength Yield Strength
23 % 27 HRC 109 ksi 98 ksi

Typical Weld Metal Analysis

OtherMnCCrFe
3.0 %2.5 %0.1 %1.5 %BAL %

x

Typical Tensile Properties

Elongation Hardness (HRC) Tensile Strength Yield Strength
23 % 27 HRC 109 ksi 98 ksi

Typical Weld Metal Analysis

OtherMnCCrFe
3.0 %2.5 %0.1 %1.5 %BAL %