Stoody ThermaClad 102'

Stoody

Stoody ThermaClad 102

Stoody ThermaClad 102

The ThermaClad 102 deposit is of modified H-12 tool steel composition. The high hardness level provides excellent abrasion resistance and will withstand high compressive loading and softening at elevated temperatures. The deposit can be applied crack free when proper welding procedures are followed. The deposit is difficult to flame cut and can be machined using carbide tools. This alloy is not recommended where resistance to fire-cracking is required. When crack-free deposits with high hardness at elevated temperatures are required ThermaClad 102 is the recommended overlay material. It exhibits good metal-to-metal and abrasion resistance.

BUY NOW


Features

  • Hardfacing overlays for: Leveler rolls, Hot work rolls, Bells seats, Dredge ladder rolls, Tool steel crane wheels.

Specifications


Typical Tensile Properties

Hardness (HRC)
51 HRC

Typical Weld Metal Analysis

OtherCCrFe
5.0 %0.5 %6.0 %BAL %

x

Typical Tensile Properties

Hardness (HRC)
51 HRC

Typical Weld Metal Analysis

OtherCCrFe
5.0 %0.5 %6.0 %BAL %