Stoody 102'

Stoody

Stoody 102

Stoody 102

Stoody 102 deposit provides excellent compressive strength along with abrasion resistance.

BUY NOW


Features

  • The maximum deposit thickness is determined by the mass of the work piece - check free deposits can be made up to 3/4" thick on 24" diameter parts without cross checking.
  • The all weld metal composition is similar to a H12 tool steel.
  • Stoody® 102 requires rigid, heavy duty equipment and carbide tools for machining. It is difficult to flame cut.


Specifications


Typical Tensile Properties

Hardness (HRC)
52 HRC

Typical Weld Metal Analysis

OtherCCrFe
6.5 %0.5 %5.5 %BAL %

x

Typical Tensile Properties

Hardness (HRC)
52 HRC

Typical Weld Metal Analysis

OtherCCrFe
6.5 %0.5 %5.5 %BAL %