Stoody ThermaClad 457
ThermaClad 457 has better resistance to tempering when compared to conventional tool steels. The deposit provides excellent abrasion resistance. It can be applied crack free with good control of preheat and interpass temperature. The combination of these properties makes this alloy ideal for applications involving high temperature and wear.
Features
- Hardfacing overlay for: Leveler rolls, Straightner rolls
Typical Tensile Properties
Deposition Data
Current | Deposition Type | Diameter | TTW Dist. | Voltage |
300-400 A | Subarc | 2.4 mm (3/32 in.) | ||
300-400 A | Full Range | 2.4 mm (3/32 in.) | 25-32 mm (1-1 1/4 in.) | 29-30 V |
380-450 A | Full Range | 3.2 mm (1/8 in.) | 32-38 mm (1 1/4-1 1/2 in.) | 30-31 V |
380-450 A | Subarc | 3.2 mm (1/8 in.) |
Typical Weld Metal Analysis %
C | Cr | Fe | Other | W |
1.0 % | 8.0 % | BAL % | 13.5 % | 5.0 % |