ThermaClad 455 has better resistance to tempering when compared to conventional tool steels. The deposit provides good abrasion resistance and can be applied crack free. ThermaClad 455 has good resistance to thermal fatigue cracking (fire cracking). The combination of these properties makes this alloy ideal for pinch roll applications.

BUY NOW


Features

  • Hardfacing overlay for: Pinch rolls, Vertical edger rolls, Straightner rolls, Hot work rolls, Piercing mill rolls, Scale breaker rolls, Hot strip rolls

Typical Tensile Properties

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
400-500 A Full Range 3.2 mm (1/8 in.) 32-38 mm (1 1/4-1 1/2 in.) 26-30 V
400-500 A Subarc 3.2 mm (1/8 in.)
450-600 A Full Range 4.0 mm (5/32 in.) 25-32 mm (1-1 1/4 in.) 28-32 V
450-600 A Subarc 2.4 mm (3/32 in.)

Typical Weld Metal Analysis %

C Cr Fe Other
0.5 % 6.0 % BAL % 4.0 %