Stoody ThermaClad 443
ThermaClad 443 deposits provide good abrasion resistance, temper resistance and can be applied crack free with appropriate welding procedures. These properties make this alloy appealing for pinch roll applications.
Features
- Hardfacing overlay for: Pinch rolls, Wrapper rolls, Vertical Edger Rolls
Typical Tensile Properties
Deposition Data
Current | Deposition Type | Diameter | TTW Dist. | Voltage |
400-500 A | Full Range | 3.2 mm (1/8 in.) | 32-38 mm (1 1/4-1 1/2 in.) | 26-30 V |
400-500 A | Subarc | 3.2 mm (1/8 in.) |
Typical Weld Metal Analysis %
C | Cr | Fe | Other |
0.50 % | 3.0 % | BAL % | 8.0 % |