Stoody ThermaClad 42

The following items have been added to your list


x

ThermaClad 42 is a new improved alloy designed for build up and overlay of undercarriage components. The alloy composition gives an optimum combination of strength, toughness.

BUY NOW


Features

  • Temper resistance and insensitivity to cooling rate.
  • It also resists metal-to-metal frictional wear.
  • Deposit hardness is approximately 40 - 42 HRC in two layers.


Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage Wire Feed Speed
400-500 A Subarc 3.2 mm (1/8 in.)
400-500 A Full Range 3.2 mm (1/8 in.) 32-38 mm (1 1/4-1 1/2 in.) 27-30 V 178-229 cm/min (70-90 in./min)

Typical Weld Metal Analysis %

C Cr Fe Other
0.2 % 2.9 % BAL % 4.0 %