Stoody ThermaClad 105B

Stoody

Stoody ThermaClad 105B

The following items have been added to your list


x

ThermaClad 105B deposit has very good resistance to metal-to-metal-wear. The deposits are readily machinable with carbide tools. Multiple layer, crack-free deposits can be obtained. When more than four layers are required, an underbase of ThermaClad 104 is recommended. Deposits are difficult to flame cut.

BUY NOW


Typical Tensile Properties

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
350-400 A Full Range 3.2 mm (1/8 in.) 25-38 mm (1-1 1/2 in.) 28-30 V
350-400 A Subarc 3.2 mm (1/8 in.)

Typical Weld Metal Analysis %

C Cr Fe Other
0.5 % 3.5 % BAL % 4.5 %
x
x
x

x

Loading..