Stoody ThermaClad 104

Stoody

Stoody ThermaClad 104

The following items have been added to your list


x

ThermaClad 104 deposit has excellent resistance to impact and plastic deformation. Deposits are machinable with high speed tools, easily machinable with carbide tools, crack-free, and can be flame cut. ThermaClad 104 is ideal for build-up and for underbase to support hardfacing. Maximum deposit thickness is unlimited.

BUY NOW


Typical Tensile Properties

ElongationTensile Strength Yield Strength
23 %750 MPa (109 ksi)675 MPa (98 ksi)

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
400-500 A Full Range 3.2 mm (1/8 in.) 32-38 mm (1 1/4-1 1/2 in.) 26-30 V
400-500 A Subarc 3.2 mm (1/8 in.)
300-400 A Full Range 2.4 mm (3/32 in.) 25-32 mm (1-1 1/4 in.) 25-29 V
450-600 A Full Range 4.0 mm (5/32 in.) 32-38 mm (1 1/4-1 1/2 in.) 28-32 V
300-400 A Subarc 2.4 mm (3/32 in.)
450-600 A Subarc 4.0 mm (5/32 in.)

Typical Weld Metal Analysis %

C Cr Fe Mn Other
0.1 % 1.5 % BAL % 2.5 % 3.0 %
x
x
x

x

Loading..