Stoody Castweld Ni 55-O/S open arc wire is used on worn cast iron parts requiring joining or build up. It has good tolerance for the high phosphorus often found in cast irons.

BUY NOW


Features

  • It works well when welding thick sections, and is also recommended for joining cast iron to dissimilar metals.
  • Castweld Ni 55-O/S can also be submerged arc welded using a neutral flux.


Typical Tensile Properties

ElongationTensile Strength Yield Strength
18 %517 MPa (75 ksi)317 MPa (46 ksi)

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
200-250 A Full Range 1.6 mm (1/16 in.) 16-19 mm (5/8-3/4 in.) 24-27 V
250-350 A Full Range 2.4 mm (3/32 in.) 19-25 mm (3/4-1 in.) 25-28 V
200-250 A Subarc 1.6 mm (1/16 in.)
250-350 A Subarc 2.4 mm (3/32 in.)

Classifications

Grade NiFeT3-CZ
Name AWS A5.15

Typical Weld Metal Analysis %

C Fe Mn Ni Si
1.0 % BAL % 3.8 % 55.0 % 0.5 %