Stoody

Stoody C-S

The following items have been added to your list


x

Stoody®C-S semi-automatic wire for submerged arc operation is a tubular nickel based wire developed for harsh environments of temperature and corrosion. The work hardening properties of this alloy make it especially resistance to metal-to-metal wear under conditions of high temperature and impact. It retains hardness up to 1200°F (650°C) and has a low coefficiency of friction. Deposits are dense and smooth.

BUY NOW


Features

  • Dense smooth deposits.
  • Especially resistant to metal-to-metal wear under high temperature and impact.
  • Nickel-based wire for submerged arc process.
  • Retains hardness up to 1200°F (650°C).
  • Hardfacing overlays for: Continuous caster rolls, Piercing mill rolls (tips), Hot forging dies, Hot trimming punches, Rotary forge hammers, Tong bits, Guide rolls, Flow controls valves.


Typical Tensile Properties

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
350-400 A Subarc 3.2 mm (1/8 in.)
350-400 A Full Range 3.2 mm (1/8 in.) 32-38 mm (1 1/4-1 1/2 in.) 28-30 V
250-300 A Full Range 2.4 mm (3/32 in.) 25-32 mm (1-1 1/4 in.) 28-30 V
250-300 A Subarc 2.4 mm (3/32 in.)

Classifications

Grade ERCNiCrMo-5A
Name AWS A5.21

Typical Weld Metal Analysis %

C Cr Fe Ni Other
0.1 % 16.0 % 5.0 % BAL % 20.0 %