Stoody 102 deposit provides excellent compressive strength along with abrasion resistance.

BUY NOW


Features

  • The maximum deposit thickness is determined by the mass of the work piece - check free deposits can be made up to 3/4" thick on 24" diameter parts without cross checking.
  • The all weld metal composition is similar to a H12 tool steel.
  • Stoody® 102 requires rigid, heavy duty equipment and carbide tools for machining. It is difficult to flame cut.


Typical Tensile Properties

Deposition Data

Current Deposition Type Diameter TTW Dist. Voltage
375-425 A Full Range 3.2 mm (1/8 in.) 25-38 mm (1-1 1/2 in.) 28-30 V
375-425 A Subarc 3.2 mm (1/8 in.)

Typical Weld Metal Analysis %

C Cr Fe Other
0.5 % 5.5 % BAL % 6.5 %