Exaton 27.7.5.L is a hyper-duplex (austenitic-ferritic) filler metal with improved yield strength and better pitting and crevice corrosion resistance compared to super-duplex stainless steels UNS S32750 and S32760. It also has higher HISC (hydrogen induced stress cracking) resistance compared to super-duplex stainless steels and higher resistance to aggressively sour environments.

Exaton 27.7.5.L can be advantageously used for welding 13% Cr flow pipes, as its high strength enables reduction of repair rates during pipeline production, because finite element analysis is not required for weld metal of matching strength and the acceptance criteria can be less conservative.

The high pitting resistance of Exaton 27.7.5.L makes it suitable for root pass welding in Exaton SAF 2507 and other super-duplex stainless steels UNS S32750 and S32760 when the risk of pitting corrosion is critical, or when mixed shielding gases cannot be used.

Exaton 27.7.5.L can also be used for overlay welding on e.g. tube sheets in heat-exchangers or for joint welding of hyper-duplex UNS S32707 pipe with wall thickness < 13 mm. It is used for TIG-welding.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded
160 J (118 ft-lb) -20 degC (-4 degF)
44 J (33 ft-lb) -50 degC (-58 degF)
190 J (141 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded27 %900 MPa (131 ksi)750 MPa (109 ksi)

Classifications

2
Grade W Z 27 7 5 L
Name EN ISO 14343-A

Consumable Characteristics

Alloy Type Austenitic-ferritic (duplex) with approx. 65% ferrite - 27% Cr - 6.5 %Ni - 5% Mo - Low C

Typical Weld Metal Analysis %

Typical Wire Composition %
C Co Cr Cu Mn Mo N Nb Ni P PRE S Si Ti V W
0.015 % 1 % 27 % 0.15 % 1.0 % 5 % 0.4 % 0.01 % 6.5 % 0.017 % 49 % 0.0007 % 0.3 % 0.001 % 0.07 % 0.02 %
Typical Weld Metal Analysis %
0.015 % 0.8 % 26.6 % 0.2 % 1.0 % 4.8 % 0.3 % 0.002 % 6.5 % 0.015 % 47 % 0.0005 % 0.3 % - 0.06 % 0.01 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton 27.7.5.L
S68916R150 FIND A DISTRIBUTOR
S68916R1X0 FIND A DISTRIBUTOR
S68920R150 FIND A DISTRIBUTOR
S68924R150 FIND A DISTRIBUTOR
S68924R1X0 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..