Due to its outstanding corrosion properties, 383 can be used in the most diverse environments, such as phosphoric and sulphuric acid, sour gas service in the oil & gas industry and chloride bearing seawater. Typical applications are found in heat exchangers, evaporators and transport piping. It is used for TIG-welding.

BUY NOW


Exaton 383

Documents


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded
140 J (104 ft-lb) -196 degC (-321 degF)
200 J (148 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded65 %540 MPa360 MPa

Classifications

Wire Electrode SFA/AWS A5.9 : ER383
EN ISO 14343-A : W 27 31 4 Cu L

Approvals

Approvals CE EN 13479
VdTÜV 02629
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Austenitic

Typical Weld Metal Analysis %

Typical Wire Composition %
Al C Co Cr Cu Mn Mo N Nb Ni P S Si
0.04 % 0.01 % 0.03 % 27.0 % 1.0 % 1.7 % 3.5 % 0.05 % 0.02 % 31.0 % 0.012 % 0.001 % 0.1 %
Typical Weld Metal Analysis %
0.03 % 0.012 % 0.04 % 26.7 % 1.1 % 1.7 % 3.5 % 0.05 % 0.01 % 30.5 % 0.01 % 0.001 % 0.05 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton 383
S65616R150 FIND A DISTRIBUTOR
S65620R150 FIND A DISTRIBUTOR
S65624R150 FIND A DISTRIBUTOR
S65632R150 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..