25.22.2.LMn is a manganese alloyed chromium-nickel-molybdenum filler material used for welding UNS S31050, 1.4466 or UNS S31603, 1.4435. The weld deposit has excellent low temperature toughness that makes it suitable for joining stainless steels for cryogenic service.
25.22.2.LMn has extensively been used successfully in all critical high-pressure units of modern urea processes, such as:
Stripper tubes - Stamicarbon, Montedison IDR
Outerlayer of bimetallic ( stripper tubes) - Saipem
Ferrules - All processes
Carbamate condensers - All processes
Decomposers - Montedison
Reactor coils - UTI
25.22.2.LMn has also found extensive use in other corrosive environments in fertilizer plants, such as:
– Nitric acid cooler/condensers cooled with polluted cooling water
– Heating coils and pipe in NPK plants – Norsk Hydro process
It is used for TIG-welding.