Exaton 25.20.L
25.20.L is a filler wire for joining UNS S31002 and similar grades used in heavily oxidizing media such as pipes in preheaters, coolers and condensers in the chemical industry. It is used for TIG-welding.

Documents
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Co | Cr | Cu | Mn | Mo | Ni | P | S | Si | |||||
<=0.020 % | <=0.20 % | 24 % | <=0.10 % | 1.8 % | <=0.30 % | 20 % | <=0.020 % | <=0.015 % | 0.2 % |
Classifications
Grade | 1.4842 |
Name | Werkstoffnummer |
Grade | G Z 25 20 L |
Name | EN ISO 14343-A |
Grade | ER"310L" |
Name | SFA/AWS A5.9 |
Typical Tensile Properties
Condition | Elongation |
As Welded | 57 % |