Documents


Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu FN WRC-92 Mn Mo N Ni P S Si
0.02 % 23.5 % 0.08 % 6 % 1.6 % 0.1 % 0.08 % 13.7 % 0.01 % 0.01 % 0.8 %
Wire Composition
<0.02 % 23.5 % <0.2 % 8 % 1.8 % 0.2 % 0.1 % 13.7 % 0.02 % 0.01 % 0.9 %

Typical Charpy V-Notch Properties

Classifications

Grade ER309LSi
Name SFA/AWS A5.9
Grade W 23 12 L Si
Name EN ISO 14343-A
Grade 1.4332
Name Werkstoffnummer

Consumable Characteristics

Alloy Type Austenitic (with approx. 9 % ferrite) 24 % Cr - 13 % Ni - Low C- High Si

Typical Tensile Properties

ConditionElongation
As Welded35 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton 309Si/309LSi
Exaton 24.13.LSi 1.2mm x 5kg S65112R150 FIND A DISTRIBUTOR
Exaton 24.13.LSi 1.6mm x 5kg S65116R150 FIND A DISTRIBUTOR
Exaton 24.13.LSi 2.0mm x 5kg S65120R150 FIND A DISTRIBUTOR
Exaton 24.13.LSi 2.4mm x 5kg S65124R150 FIND A DISTRIBUTOR
Exaton 24.13.LSi 3.2mm x 5kg S65132R150 FIND A DISTRIBUTOR