Exaton 309L HF
309L HF welding wire is used for TIG, plasma-arc, MIG and submerged-arc welding. It is particularly suitable for overlay welding and joining dissimilar steels, for example austenitic stainless steels to low alloyed or non alloyed steels. It has excellent resistance to hot cracking due to its enhanced ferrite content.It is used for TIG-welding.

Documents
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Co | Cr | Cu | Mn | Mo | N | Ni | P | S | Si | ||||
<=0.015 % | <=0.05 % | 24 % | <=0.10 % | 1.8 % | <=0.3 % | <0.06 % | 13 % | <=0.015 % | <=0.015 % | 0.3 % |
Approvals
Society | CE |
Grade | EN 13479 |
Approvals are based on factory location. Please contact ESAB for more information. |
Classifications
Grade | ER309L |
Name | SFA/AWS A5.9 |
Grade | W 23 12 L |
Name | EN ISO 14343-A |
Grade | 1.4332 |
Name | Werkstoffnummer |
Typical Tensile Properties
Condition | Elongation |
As Welded | 71 % |