Exaton 309/309L
309/309L is suitable for joining stainless Cr-Ni steels of the 309 type, Cr-steels and dissimilar steels e.g. austenitic stainless steel to carbon or low-alloyed steels for service up to 320°C (610°F). Widely used as barrier layer between carbon/low alloy steel and different stainless grades in cladding operations. It is used for TIG-welding.

Documents
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Co | Cr | Cu | FN WRC-92 | Mn | Mo | N | Nb | Ni | P | S | Si | V | |
0.01 % | 0.03 % | 23.5 % | 0.04 % | 12 % | 1.67 % | 0.04 % | 0.08 % | 0.01 % | 13 % | 0.018 % | 0.014 % | 0.40 % | 0.03 % | |
Wire Composition | ||||||||||||||
<0.02 % | - | 23.5 % | <0.1 % | 10 % | 1.8 % | <0.1 % | 0.08 % | - | 13.5 % | 0.01 % | 0.01 % | 0.4 % | - |
Approvals
Society | CE |
Grade | EN 13479 |
Approvals are based on factory location. Please contact ESAB for more information. |