Exaton

Exaton 2209

The following items have been added to your list


x

2209 is used for welding of duplex stainless steels such as 2205 and 2304. It can also be used for welding of duplex stainless steels to carbon steel. It is used for TIG-welding.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded
180 J (133 ft-lb) -20 degC (-4 degF)
160 J (118 ft-lb) -40 degC (-40 degF)
155 J (115 ft-lb) -46 degC (-51 degF)
145 J (107 ft-lb) -50 degC (-58 degF)
200 J (148 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded28 %710 MPa (103 ksi)580 MPa (84 ksi)

Classifications

Wire Electrode SFA/AWS A5.9 : ER2209
EN ISO 14343-A : W 22 9 3 N L
EN ISO 14343-B : 2209

Approvals

Approvals ABS ER 2209
BV ER 2209
CE EN 13479
DNV-GL Duplex Steels
VdTÜV 19480
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Austenitic-ferritic (duplex) with approx. 55 FN ferrite - 22.5% Cr - 8% Ni - 3% Mo - Low C

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Co Cr Cu FN WRC-92 Mn Mo N Nb Ni P PRE S Si Ti V W
0.01 % - 23 % 0.1 % 54 % 1.5 % 3.1 % 0.16 % 0.01 % 8.5 % 0.02 % 35.8 % 0.001 % 0.5 % - - 0.01 %
Typical Wire Composition %
0.012 % 0.04 % 23 % 0.09 % 55 % 1.5 % 3.2 % 0.15 % 0.01 % 8.6 % 0.018 % 37 % 0.0007 % 0.5 % 0.003 % 0.05 % 0.01 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton 2209
S68612R150 FIND A DISTRIBUTOR
S68616R150 FIND A DISTRIBUTOR
S68620R150 FIND A DISTRIBUTOR
S68624R150 FIND A DISTRIBUTOR
S68632R150 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..