Exaton 22.15.3.L
22.15.3.L is an austenitic filler material for joining stainless steels to carbon steels or low-alloy steels and for overlay welding. It is used for TIG-welding.

Documents
Typical Charpy V-Notch Properties
Impact Value | Testing Temperature |
140 J | 20 degC |
30 J | -196 degC |
Classifications
Wire Electrode |
EN ISO 14343-A : W 23 12 2 L SFA/AWS A5.9 : ER(309LMo) EN 10088-1 : ~1.4435 |
Typical Tensile Properties
Condition | As Welded | As Welded | As Welded |
Shielding Gas | AWS | ISO | |
Tensile Strength | 630 MPa | ||
Yield Strength | 515 MPa | ||
Elongation | 26 % | ||