Exaton

Exaton 385

The following items have been added to your list


x

385 welding wire is suitable for joining steels of the 20Cr/25Ni/4.5Mo/1.5Cu type - for example 904L (e.g. 2RK65) used in many areas of the process industry, such as in the production of acetic acid, sulfuric acid, terephthalic or tartaric acid and vinyl chloride. It is also suitable for use in cooling operations involving sea water or heavily polluted river water. It is used for TIG-welding.

BUY NOW


Exaton 385

Documents


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded
100 J (74 ft-lb) -196 degC (-321 degF)
120 J (89 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded60 %540 MPa (78 ksi)320 MPa (46 ksi)

Classifications

Wire Electrode SFA/AWS A5.9 : ER385
EN ISO 14343-A : W 20 25 5 Cu L
Werkstoffnummer : 1.4519

Approvals

Approvals CE EN 13479
VdTÜV 02223
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cr Cu Mn Mo Ni P S Si
<=0.020 % 20 % 1.5 % 1.8 % 4.5 % 25 % <=0.015 % <=0.015 % 0.4 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton 385
S65516R150 FIND A DISTRIBUTOR
S65520R150 FIND A DISTRIBUTOR
S65524R150 FIND A DISTRIBUTOR
S65532R150 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.