Exaton NiCr-3
NiCr-3 is filler material for joining NiCrFe alloys, 9% Ni steels used at cryogenic temperatures, stainless steels to carbon steels, high service temperature NiCu alloys to carbon steels and NiCu alloys to nickel alloys. NiCr-3 can be used in air up to 1175°C (2145°F) and in sulphur dioxide atmospheres up to 800°C (1470°F). NiCr-3 is suitable for MIG, TIG, PAW and SAW and available as wire and rods. It is used for TIG-welding.

Documents
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||||
Al | C | Co | Cr | Cu | Fe | Mn | Mo | N | Nb | Nb+Ta | Ni | P | S | Si | Ti | |
0.4 % | <=0.03 % | <=0.1 % | 20 % | <=0.05 % | <=1 % | 3 % | ≤0.05 % | <=0.05 % | ≤0.05 % | 2.5 % | 2.6 % | 73 % | <=0.01 % | <=0.01 % | 0.1 % | 0.4 % |
Typical Weld Metal Analysis % | ||||||||||||||||
- | <0.02 % | <0.02 % | 20 % | 0.01 % | ≤1 % | 3.2 % | 0.01 % | 0.03 % | 2.2 % | 2.5 % | 73 % | <0.003 % | 0.003 % | 0.01 % | 0.4 % |
Approvals
Society | CE |
Grade | EN 13479 |
Approvals are based on factory location. Please contact ESAB for more information. |
Typical Charpy V-Notch Properties
Classifications
Grade | ERNiCr-3 |
Name | SFA/AWS A5.14 |
Grade | S Ni 6082 (NiCr20Mn3Nb) |
Name | EN ISO 18274 |
Typical Tensile Properties
Condition | Elongation |
As Welded | 35 % |