NiCrMo-4 is a low carbon nickel-chrome-molybdenum alloy of type alloy C-276. It is a versatile alloy with excellent wet corrosion resistance in oxidizing and especially in reducing media. However, in oxidizing chloride containing environments alloy UNS N06022 (2.4602) is preferred where NiCrMo-10 is a better matching welding consumable. Applications for NiCrMo-4 are found in aggressively corrosive media such as chemical processing plants, pollution control, pulp and paper production, waste treatment and for the recovery of sour natural gas. NiCrMo-4 is used for joining alloy UNS N10276 (2.4819) and other nickel-chrome-molybdenum alloys. It can also be used for dissimilar metal joining of nickel alloys, stainless steels and low-alloy steels. NiCrMo-4 can be used for surfacing low alloyed steels. Applications for NiCrMo-4 are found in cryogenics, components in pulp and paper plants such as bleaching vessels, flue gas scrubber systems, components in sour-gas service, sulphuric acid coolers, chlorine gas, hypochlorite and chlorine dioxide atmosphere. NiCrMo-4 is also used in combustion-resistant components for high pressure oxygen service.It is used for TIG welding.

BUY NOW


Exaton NiCrMo-4

Documents


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded
130 J (96 ft-lb) -196 degC (-321 degF)
170 J (126 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded45 %750 MPa (109 ksi)470 MPa (68 ksi)

Classifications

Wire Electrode SFA/AWS A5.14 : ERNiCrMo-4
EN ISO 18274 : S Ni 6276 (NiCr15Mo16Fe6W4)
Werkstoffnummer : 2.4819

Approvals

Grade EN 13479
Society CE
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Wire Composition %
C Co Cr Fe Mn Mo Ni P S Si V W
<=0.02 % <=2.5 % 16 % 5 % <=1 % 16 % 56 % <=0.03 % <=0.03 % <=0.08 % <0.35 % 3.5 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton NiCrMo-4
S98316R150 FIND A DISTRIBUTOR
S98320R150 FIND A DISTRIBUTOR
S98324R150 FIND A DISTRIBUTOR
S98332R150 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..