NiCrMo-10 is a nickel-chrome-molybdenum alloy of type alloy C-22. It is a versatile alloy with excellent wet corrosion resistance in oxidizing and reducing media. It has better overall corrosion resistance than other Ni-Cr-Mo alloys such as alloy UNS N10276 (2.4819) and alloy UNS N06626 (2.4856). However, in severely reducing media alloy UNS N10276 is preferred where NiCrMo-10 is a better matching consumable. Applications for NiCrMo-10 are found in aggressively corrosive media such as chlorination systems, geothermal wells, HF furnace scrubbers, pesticide production, phosphoric acid production, SO cooling towers and for weld overlays on valves. NiCrMo-10 is used for joining alloy UNS N06022 (2.4602) and is widely used as overmatching filler material for alloy UNS N10276 (2.4819) and other nickel-chrome-molybdenum alloys for better weld metal properties. It is used for surfacing low alloyed steels. Applications for NiCrMo-10 are found in components for organic synthesis, flue gas scrubber systems, electrolytic galvanizing, plate heat exchangers, phosphoric acid production, wet chlorine gas, hypochlorite and chlorine dioxide atmosphere. NiCrMo-10 is also used in combustion-resistant components for high pressure oxygen service and ferric and cupric chloride environments.It is used for TIG welding.

BUY NOW


Exaton NiCrMo-10

Documents


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded
80 J (59 ft-lb) -196 degC (-321 degF)
150 J (111 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded50 %770 MPa (112 ksi)500 MPa (73 ksi)

Classifications

Wire Electrode SFA/AWS A5.14 : ERNiCrMo-10
Werkstoffnummer : 2.4602
EN ISO 18274 : S Ni 6022 (NiCr21Mo13Fe4W3)

Approvals

Grade EN 13479
Society CE
Approvals are based on factory location. Please contact ESAB for more information.

Typical Weld Metal Analysis %

Typical Wire Composition %
C Co Cr Fe Mn Mo Ni P S Si V W
<=0.015 % <=2.5 % 21.5 % <=4 % <=0.50 % 13.5 % 56 % <=0.020 % <=0.010 % <=0.08 % <=0.35 % 3 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton NiCrMo-10
S98716R150 FIND A DISTRIBUTOR
S98724R150 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..