Exaton

Exaton NiCr-3

The following items have been added to your list


x

NiCr-3 welding wire is suitable for overlay welding when a deposit with chemistry corresponding to UNS N08825 is required. The weld deposit is a nickel-iron-chromium-molybdenum-copper alloy suitable for use in extremely corrosive environments. NiCr-3 has very good resistance to stress corrosion cracking (SCC) in chloride containing environments and is particularly suited for use in reducing environments such as those containing sulphuric and phosphoric acids. NiCr-3 is used for corrosion resistant alloy surfacing of components in the chemical, pollution control, oil & gas and petrochemical industries and often in connection with sour gas service. Typical components are tanks, heat exchangers, evaporators, transport pipes and scrubbers etc. It is used for TIG welding.

BUY NOW


Exaton NiCr-3

Documents


Typical Tensile Properties

ConditionTensile Strength Yield Strength
As Welded550 MPa (80 ksi)340 MPa (49 ksi)

Classifications

Wire Electrode SFA/AWS A5.14 : ERNiFeCr-1
EN ISO 18274 : S Ni 8065 (NiFe30Cr21Mo3)

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cr Cu Fe Mn Mo Ni P S Si
<=0.025 % 23 % 2.3 % >=22.0 % 1 % 3 % >=42.0 % <=0.025 % <=0.010 % <=0.3 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton NiCr-3
S99016R150 FIND A DISTRIBUTOR
S99020R150 FIND A DISTRIBUTOR
S99024R150 FIND A DISTRIBUTOR