Exaton 35WF
Exaton 35WF is a basic welding flux for submerged arc welding giving good slag removal and a fine bead appearance. Its relatively high basicity makes it suitable for joining of the austenitic and duplex stainless steel when high impact strength is desired. Due to its low niobium content burn-off it can be used advantageously with stabilized wire electrodes.
Exaton 35WF is a high performance welding flux in many joining applications in the chemical, petrochemical and oil & gas industry. It is particularly suited for Exaton range of duplex wire electrodes (e.g. 22.8.3.L/25.10.4.L) due to the highly neutral behavior, which ensures an optimal balanced microstructure.

Documents
Classifications
Grade | S A AF 2 |
Name | EN ISO 14174 |
Consumable Characteristics
Basicity Index | nom: 1.9 % |
Density | nom: 1.0 Kg/l |
Slag Type | Fluoride basic CaF2-Al2O3-SiO2 |
Welding Current | 1200 A (Using 60x0.5 mm strip) |
Flux Consumption
Volts | kg Flux / kg Wire DC+ |
26 V | 0.5 kg |
30 V | 0.6 kg |
34 V | 0.8 kg |
38 V | 1.0 kg |
Amps | Dimensions | Travel speed |
580 A | 4.0 mm | 33 m/h |
Classifications
Wire | AWS/EN |
Exaton 19.9 | A5.9:ER308/308H/ 14343-A:S 19 9 H |
Exaton 19.12.3.LCRYO | A5.9:ER316L/ 14343-A:S 19 12 3 L |
Approvals
Wire |
*Selected production units only. Please contact ESAB for more information. Visit esab.com to download specific flux/wire combination fact sheets for more details. |
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||
C | Cr | Mn | Mo | N | Ni | P | S | Si | Si+Fe | |||||
Exaton 19.12.3.LCRYO | ||||||||||||||
0.021 % | 18 % | 1.5 % | 2.3 % | 0.06 % | 12.8 % | 0.023 % | 0.003 % | 0.5 % | 3 % |