Exaton 22.12.HT
Exaton 22.12.HT is an austenitic filler material for welding the high temperature steel grade Sandvik 253 MA*, UNS S30815. It is characterized by high creep strength, good resistance to oxidation and good weldability.
* 253 MA is a trademark owned by Outokumpu OY. It is used for Submerged Arc Welding.

Documents
Classifications
Wire Electrode |
Werkstoffnummer : 1.4829 EN ISO 14343-A : S Z 21 10 N |
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Ce | Cr | Cu | Mn | Mo | N | Ni | P | S | Si | ||||
0.08 % | 0.06 % | 21 % | 0.18 % | 0.5 % | <=0.3 % | 0.17 % | 10 % | <=0.025 % | <=0.015 % | 1.6 % |