Exaton 19.9.Nb HF

Exaton

Exaton 19.9.Nb HF

The following items have been added to your list


x

Exaton 19.9.Nb HF (High Ferrite) is a variant of the most common 19.9.Nb, but with a higher ferrite value. Its chemical composition is designed for tough applications, for example when a post weld heat treatment is required.

The recommended flux is Exaton 15W; however, Exaton 19.9.Nb HF can also be used in combination with other fluxes.

BUY NOW


Classifications

Wire Electrode EN ISO 14343-A : S 19 9 Nb
SFA/AWS A5.9 : ER347

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cr Cu FN WRC FN deLong Mn Mo N Nb Nb+Ta Ni P S Si
0.045 % 19.8 % 0.11 % 12 % 13 % 1.8 % 0.12 % 0.03 % 0.7 % 0.7 % 9.3 % 0.02 % 0.01 % 0.49 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton 19.9.Nb HF
SF21240400 FIND A DISTRIBUTOR
SF21243110 FIND A DISTRIBUTOR
SF21323110 FIND A DISTRIBUTOR
SF21320400 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..