Exaton 22.12.HT is an austenitic filler material for welding the high temperature steel grade Sandvik 253 MA*, UNS S30815. It is characterized by high creep strength, good resistance to oxidation and good weldability.

* 253 MA is a trademark owned by Outokumpu OY. It is used for Submerged Arc Welding.

BUY NOW


Exaton 22.12.HT

Documents


Typical Weld Metal Analysis %

Wire Composition
C Ce Cr Cu Mn Mo N Ni P S Si
0.08 % 0.06 % 21 % 0.18 % 0.5 % <=0.3 % 0.17 % 10 % <=0.025 % <=0.015 % 1.6 %

Classifications

Grade 1.4829
Name Werkstoffnummer
Grade S Z 21 10 N
Name EN ISO 14343-A