385 welding wire is suitable for joining steels of the 20Cr/25Ni/4.5Mo/1.5Cu type - for example 904L used in many areas of the process industry, such as in the production of acetic acid, sulfuric acid, terephthalic or tartaric acid and vinyl chloride. It is also suitable for use in cooling operations involving sea water or heavily polluted river water. It is used for Submerged Arc Welding.

BUY NOW


Exaton 385

Documents


Typical Weld Metal Analysis %

Wire Composition
C Cr Cu Mn Mo Ni P S Si
<=0.020 % 20 % 1.5 % 1.8 % 4.5 % 25 % <=0.015 % <=0.015 % 0.4 %

Approvals

Society CE
Grade EN 13479
Approvals are based on factory location. Please contact ESAB for more information.

Classifications

Grade ER385
Name SFA/AWS A5.9
Grade S 20 25 5 Cu L
Name EN ISO 14343-A
Grade 1.4519
Name Werkstoffnummer
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton 385
Exaton 20.25.5.LCu 2.0mmX25kg S655203110 FIND A DISTRIBUTOR
Exaton 20.25.5.LCu 2.4mmX25kg S655243110 FIND A DISTRIBUTOR
Exaton 20.25.5.LCU 3.2mm 25kg S655323110 FIND A DISTRIBUTOR
x
x

x

Loading..