Exaton Ni56 is a nickel-chromium-molybdenum strip electrode designed for electroslag welding (ESW) to deposit a second layer corrosion resistant alloy of Ni 6276/UNS N10276 composition on carbon and low alloyed steels. The recommended flux is Exaton 69S; however, Exaton Ni56 can also be used in combination with other fluxes.

BUY NOW


Classifications

Classifications SFA/AWS A5.14 : EQNiCrMo-4
EN ISO 18274 : B Ni6276 (NiCr15Mo16Fe6W4)

Consumable Characteristics

Alloy Type EQNiCrMo-4

Typical Weld Metal Analysis %

Typical Wire Composition %
C Co Cr Cu Fe Mn Mo Ni P S Si V W
<=0.02 % <0.1 % 16 % <0.1 % 5 % 0.2 % 16 % >=50 % <0.01 % <0.01 % 0.05 % <0.05 % 4 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton Ni56
S198530200 FIND A DISTRIBUTOR
S198560200 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..