Exaton 15W is a basic welding flux for submerged arc welding giving good slag removal and a fine bead appearance. Its relatively high basicity makes it suitable for joining of austenitic and duplex stainless steel when high impact strength is desired. Due to its low niobium content burn-off it can be used advantageously with stabilized wire electrodes.

Exaton 15W is a high performance welding flux in many joining applications in the chemical, petrochemical and oil&gas industry. It is particularly suited for Exaton range of duplex wire electrodes (e.g. 22.8.3.L/25.10.4.L) due to the highly neutral behavior, which ensures an optimal balanced microstructure.

Taking the benefit of its features (not limited to nice bead appearance and self slag release only), it can also be used in combination with NiCrMo-3 wire for several other applications (i.e. both joining and weld overlay).

BUY NOW


Specifications


Approvals

Society Wire
DNV 25.10.4.L SAW
VdTÜV 25.10.4.L SAW

Classifications

AWS/EN Wire
A5.9:ER2594/ 14343:25 9 4 N L 25.10.4.L SAW

Flux Consumption

Amps Dimensions kg Flux / kg Wire DC+ Travel speed Volts
580 A 4.0 mm 0.5 kg 33 m/h 26 V
580 A 4.0 mm - 33 m/h 26 V
580 A 4.0 mm 0.6 kg 33 m/h 30 V
580 A 4.0 mm - 33 m/h 30 V
580 A 4.0 mm 0.8 kg 33 m/h 34 V
580 A 4.0 mm - 33 m/h 34 V
580 A 4.0 mm 1.0 kg 33 m/h 38 V
580 A 4.0 mm - 33 m/h 38 V

Typical Mechanical Properties

Charpy V-Notch Charpy V-Notch Testing Temp Condition Elongation Tensile Strength Wire Yield Strength
90 J 20 °C As Welded 25 % 880 MPa 25.10.4.L SAW 690 MPa
60 J -40 °C As Welded 25 % 880 MPa 25.10.4.L SAW 690 MPa

Typical Weld Metal Analysis

weld metal analysis
PMnMoCSSiNiNCr
<=0.020 %0.3 %4 %<=0.020 %<=0.015 %0.6 %9.6 %0.21 %24.5 %

Classifications: EN ISO 14174; S A AF 2

Basicity Index: nom: 1.9
Density: nom: 1.0 Kg/l
Slag Type: Fluoride basic CaF2-Al2O3-SiO2
Welding Current: METRIC_1200 A (Using 60x0.5 mm strip)
x
Exaton 15W

Approvals

Society Wire
DNV 25.10.4.L SAW
VdTÜV 25.10.4.L SAW

Classifications

AWS/EN Wire
A5.9:ER2594/ 14343:25 9 4 N L 25.10.4.L SAW

Flux Consumption

Amps Dimensions kg Flux / kg Wire DC+ Travel speed Volts
580 A 4.0 mm 0.5 kg 33 m/h 26 V
580 A 4.0 mm - 33 m/h 26 V
580 A 4.0 mm 0.6 kg 33 m/h 30 V
580 A 4.0 mm - 33 m/h 30 V
580 A 4.0 mm 0.8 kg 33 m/h 34 V
580 A 4.0 mm - 33 m/h 34 V
580 A 4.0 mm 1.0 kg 33 m/h 38 V
580 A 4.0 mm - 33 m/h 38 V

Typical Mechanical Properties

Charpy V-Notch Charpy V-Notch Testing Temp Condition Elongation Tensile Strength Wire Yield Strength
90 J 20 °C As Welded 25 % 880 MPa 25.10.4.L SAW 690 MPa
60 J -40 °C As Welded 25 % 880 MPa 25.10.4.L SAW 690 MPa

Typical Weld Metal Analysis

weld metal analysis
PMnMoCSSiNiNCr
<=0.020 %0.3 %4 %<=0.020 %<=0.015 %0.6 %9.6 %0.21 %24.5 %

Classifications: EN ISO 14174; S A AF 2

Basicity Index: nom: 1.9
Density: nom: 1.0 Kg/l
Slag Type: Fluoride basic CaF2-Al2O3-SiO2
Welding Current: METRIC_1200 A (Using 60x0.5 mm strip)
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton 15W
Exaton 15W 25kg bucket S128400000 FIND A DISTRIBUTOR
Exaton 15W 25kg bucket S12840000F FIND A DISTRIBUTOR
Exaton 15W 20kg bucket S128S02000 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..