Exaton SX
SX is a filler wire for joining SX steel (UNS S32615, ASME Code Case 2029-3) used in concentrated sulfuric acid. It is used for MIG/MAG welding.

Documents
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Cr | Cu | Mn | Ni | P | S | Si | |||||||
<=0.018 % | 18.5 % | 2 % | 1.7 % | 13.5 % | <=0.015 % | <=0.005 % | 5 % |
Classifications
Name | EN ISO 14343-A |
Grade | G Z 18 13 L |
2 |
Typical Tensile Properties
Condition | Elongation |
As Welded | 55 % |
Deposition Data
Wire Feed Speed | 0.0-0.0 m/min |
Voltage | 25-30 V |
Diameter | 1.6 mm |
Deposition Rate | 0.0-0.0 kg/h |
Current | 230-350 A |