Exaton AXT
Exaton AXT is a filler metal with increased manganese content, reducing the risk for fissuring / hot cracking that otherwise can be a problem in fully austenitic weld metals. It is suitable for joining work-hardenable steels, armor plates, austenitic stainless manganese steels and stainless cr steels with max 18% Cr.

Documents
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Cr | Cu | Mn | Mo | N | Ni | P | S | Si | |||||
0.08 % | 18 % | <=0.1 % | 7 % | <=0.3 % | <=0.06 % | 8 % | <=0.025 % | <=0.015 % | 0.9 % |
Approvals
Society | CE |
Grade | EN 13479 |
Approvals are based on factory location. Please contact ESAB for more information. |
Classifications
Grade | ER(307) modified |
Name | SFA/AWS A5.9 |
Grade | G 18 8 Mn |
Name | EN ISO 14343 |
Typical Tensile Properties
Condition | Elongation |
As Welded | 41 % |