29.8.2.L is used for MIG/MAG welding of the super-duplex grade Sandvik SAF 2906. Typical applications are welding of piping systems in Caustic soda production as well as welding of pipes and heat ex-changers in Alumina production.

BUY NOW


Typical Charpy V-Notch Properties

As Welded
Impact Value 150 J
Testing Temperature 20 °C

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded25 %880 MPa670 MPa

Classifications

2
Grade G Z 29 8 2 L
Name EN ISO 14343-A

Typical Weld Metal Analysis %

Typical Wire Composition %
C Co Cr Cu Mn Mo N Nb Ni P PRE S Si Ti
<0.025 % 0.07 % 29 % 0.11 % 1.0 % 2.2 % 0.3 % 0.01 % 7 % 0.015 % 41.7 % 0.0005 % 0.4 % 0.003 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton 29.8.2.L
S669119820 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..