309LNb is a niobium-stabilized overalloyed filler metal suitable for overlay welding of carbon and low alloy steels, where a type 347 of overlay is required. It is used for MIG/MAG welding.

Documents
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Cr | Mn | Nb | Ni | P | S | Si | |||||||
<=0.020 % | 24 % | 2 % | 0.8 % | 12.5 % | <=0.020 % | <=0.015 % | 0.3 % |