2209 is used for welding of duplex stainless steels such as 2205 and 2304. It can also be used for welding of duplex stainless steels to carbon steel. It is used for MIG/MAG welding.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded
105 J (78 ft-lb) -20 degC (-4 degF)
100 J (74 ft-lb) -40 degC (-40 degF)
95 J (70 ft-lb) -46 degC (-51 degF)
90 J (67 ft-lb) -50 degC (-58 degF)
110 J (81 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded30 %770 MPa (112 ksi)550 MPa (80 ksi)

Recommended Welding Parameters

Current Voltage Wire Diameter Wire Feed Speed
40-120 A 15-19 V 0.8 mm (0.030 in.) 4.0-8.0 m/min (157-315 in./min)
60-220 A 15-28 V 1.0 mm (0.040 in.) 4.0-12.0 m/min (157-472 in./min)
150-260 A 24-29 V 1.2 mm (0.047 in.) 3.0-10.0 m/min (118-394 in./min)
230-350 A 25-30 V 1.6 mm (1/16 in.) 3.0-5.0 m/min (118-197 in./min)

Classifications

Wire Electrode EN ISO 14343-A : G 22 9 3 N L
SFA/AWS A5.9 : ER2209
EN ISO 14343-B : 2209

Approvals

Approvals CE EN 13479
DNV-GL Stainless steel*
VdTÜV 19479
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Austenitic-ferritic (duplex) with approx. 55 FN ferrite - 22.5% Cr - 8% Ni - 3% Mo - Low C

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Co Cr Cu FN WRC-92 Mn Mo N Nb Ni P PRE S Si Ti V W
0.014 % - 23 % 0.09 % 52 % 1.5 % 3.0 % 0.15 % 0.01 % 8.5 % 0.017 % 35.3 % 0.001 % 0.45 % - - 0.01 %
Typical Wire Composition %
0.012 % 0.04 % 23 % 0.09 % 55 % 1.5 % 3.2 % 0.15 % 0.01 % 8.6 % 0.018 % 37 % 0.0007 % 0.5 % 0.003 % 0.05 % 0.01 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton 2209
S686084600 FIND A DISTRIBUTOR
S686089820 FIND A DISTRIBUTOR
S686082110 FIND A DISTRIBUTOR
S68610982W FIND A DISTRIBUTOR
S686103820 FIND A DISTRIBUTOR
S686103400 FIND A DISTRIBUTOR
S686109820 FIND A DISTRIBUTOR
S686109320 FIND A DISTRIBUTOR
S68612982W FIND A DISTRIBUTOR
S686123820 FIND A DISTRIBUTOR
S686123800 FIND A DISTRIBUTOR
S686123400 FIND A DISTRIBUTOR
S686129820 FIND A DISTRIBUTOR
S686129320 FIND A DISTRIBUTOR
S686163820 FIND A DISTRIBUTOR
S686163800 FIND A DISTRIBUTOR
S686169820 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..