Exaton 309LMo
22.15.3.L is an austenitic filler material for joining stainless steels to carbon steels or low-alloy steels and for overlay welding. It is used for MIG/MAG welding.

Documents
Typical Charpy V-Notch Properties
Impact Value | Testing Temperature |
95 J | 20 degC |
20 J | -196 degC |
Classifications
Wire Electrode |
EN ISO 14343-A : G 23 12 2 L SFA/AWS A5.9 : ER(309LMo) EN 10088-1 : ~1.4435 |
Typical Tensile Properties
Condition | As Welded | As Welded | As Welded |
Shielding Gas | AWS | ISO | |
Tensile Strength | 610 MPa | ||
Yield Strength | 450 MPa | ||
Elongation | 31 % | ||
Deposition Data
Current | Deposition Rate | Diameter | Voltage | Wire Feed Speed |
40-120 A | 0.0-0.0 kg/h(0-0 lb/h) | 0.8 mm(0.030 in.) | 15-19 V | 4.0-4.0 m/min(157-157 in./min) |
150-260 A | 0.0-0.0 kg/h(0-0 lb/h) | 1.2 mm(0.047 in.) | 24-29 V | 3.0-3.0 m/min(118-118 in./min) |
230-350 A | 0.0-0.0 kg/h(0-0 lb/h) | 1.6 mm(1/16 in.) | 25-30 V | 3.0-3.0 m/min(118-118 in./min) |