308/308L (CRYO) is a filler material for joining austenitic stainless steels, e.g. ASTM 304, 304L (18Cr/8Ni/ELC), for cryogenic applications and meets the requirements of ASME Section VIII, Division 1, UHA 51 ((a) (4) (-a) (-1)) and others. It is also used for service temperatures down to -269°C (-452°F), and ferritic or martensitic stainless steels with maximum 19% Cr. 308/308L (CRYO) is approved by TÜV Rheinland for use at cryogenic temperatures down to 4K (-269°C (-452°F). It is suitable for joining stainless steels of 18Cr/8Ni/Nb types, e.g. ASTM 347, for service temperatures up to 350°C (660°F). It is used for MIG/MAG welding. Specifically developed for welding in cryogenic applications, typically: manufacturing of dewars, containers, tanks, cryostats, and transfer systems for transportation and storage of LNG, LPG, liquid nitrogen and liquid helium. The chemical composition is optimized for cryogenic applications in terms of impact strength and other characteristics. It has a controlled chemical composition and ferrite content for resistance to microfissuring, and balanced minor additions of certain elements for optimum arc stability, fluidity and low spatter.

BUY NOW


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 38 % 610 MPa 460 MPa
As Welded 25 % 440 MPa 290 MPa

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 150 J 20 °C
As Welded 80 J -196 °C
As Welded 40 J -269 °C

Typical Weld Metal Analysis

weld metal analysis
MnMoCFN WRC-92CoNCrPCuSNbTiSiNi
1.9 %0.3 %0.011 %6 %0.05 %0.06 %19.6 %0.018 %0.15 %0.008 %0.01 %0.003 %0.3 %10.1 %
wire composition
MnMoCFN WRC-92CoNCrPCuSNbTiSiNi
1.8 %0.2 %0.010 %6 %0.10 %0.05 %19.8 %0.020 %0.2 %0.009 %0.01 %0.003 %0.4 %10.8 %

Approvals: CE; EN 13479
Classifications: EN ISO 14343-A; G 19 9 L; Wire Electrode; SFA/AWS A5.9; ER308L; Wire Electrode; Werkstoffnummer; 1.4316; Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


x
Exaton 308/308L (CRYO)

Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 38 % 610 MPa 460 MPa
As Welded 25 % 440 MPa 290 MPa

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 150 J 20 °C
As Welded 80 J -196 °C
As Welded 40 J -269 °C

Typical Weld Metal Analysis

weld metal analysis
MnMoCFN WRC-92CoNCrPCuSNbTiSiNi
1.9 %0.3 %0.011 %6 %0.05 %0.06 %19.6 %0.018 %0.15 %0.008 %0.01 %0.003 %0.3 %10.1 %
wire composition
MnMoCFN WRC-92CoNCrPCuSNbTiSiNi
1.8 %0.2 %0.010 %6 %0.10 %0.05 %19.8 %0.020 %0.2 %0.009 %0.01 %0.003 %0.4 %10.8 %

Approvals: CE; EN 13479
Classifications: EN ISO 14343-A; G 19 9 L; Wire Electrode; SFA/AWS A5.9; ER308L; Wire Electrode; Werkstoffnummer; 1.4316; Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton 308/308L (CRYO)
Exaton 19.9.LCRYO 1.0mm X 15kg SF10109820 FIND A DISTRIBUTOR
Exaton 19.9.LCRYO 1.2mm X 15kg SF10129820 FIND A DISTRIBUTOR
Exaton 19.9.LCRYO 1.6mm X 15kg SF10169820 FIND A DISTRIBUTOR