Exaton 19.12.3.LSiMo
Exaton 19.12.3.LSiMo is used for welding of austenitic stainless alloys of 18% Cr - 8% Ni and 18% Cr - 10% Ni - 3% Mo-types, stabilized or non-stabilized, e.g. ASTM 316, 316L and 316Ti as well as 304, 304L, 321 and 347, for service temperatures up to 400°C (750°F). It is also used for welding of stainless Cr-steels with max 19% Cr. Exaton 19.12.3.LSiMo is particularly suited for GMAW, but can also be used for automated GTAW and plasma welding. The critical pitting temperature, CPT, according to ASTM G150 (1°C of accuracy) can be as high as 39°C compared to standard 316LSi, which achieved maximum 29°C during the benchmark. The results were achieved with GMAW, but are expected to be on the same level or better for GTAW.

Documents
Typical Charpy V-Notch Properties
as welded | ||||
Classifications
Wire Electrode |
Werkstoffnummer : ~1.4430 EN ISO 14343-A : W 19 12 3 L Si SFA/AWS A5.9 : 316LSi |
Approvals
Grade | EN 13479 |
Society | CE |
Approvals are based on factory location. Please contact ESAB for more information. |
Consumable Characteristics
Alloy Type | Austenitic (with appr. 9 % ferrite) 19 % Cr - 12 % Ni - 3 % Mo - Low C - High Si |
Shielding Gas | I1 (EN ISO 14175) |
Typical Weld Metal Analysis %
Typical Wire Composition % | ||||||||||||||
C | Co | Cr | Cu | FN WRC-92 | Mn | Mo | N | Nb | Ni | P | S | Si | Ti | |
0.013 % | 0.05 % | 18.5 % | 0.10 % | 9 % | 1.8 % | 2.9 % | 0.05 % | 0.04 % | 12 % | 0.018 % | 0.010 % | 0.9 % | 0.002 % | |
Typical Weld Metal Analysis % | ||||||||||||||
0.01 % | 0.05 % | 18.8 % | 0.1 % | 9 % | 1.8 % | 2.8 % | 0.06 % | 0.02 % | 12 % | 0.017 % | 0.007 % | 0.9 % | - |