Exaton

Exaton 316L Cryo

The following items have been added to your list


x

316L Cryo is a filler material for joining austenitic stainless steels, e.g. ASTM 316, 316L, as well as 304, 304L, for cryogenic applications and meets the requirements of ASME Section VIII, Division 1, UHA 51 ((a) (4) (-a) (-1)) and others. It is used for service temperatures down to -269ºC (-452ºF), and ferritic or martensitic stainless steels, with maximum 19% Cr. It is used for MIG/MAG welding. The grade has been specifically developed for welding in cryogenic applications, typically: manufacturing of dewars, containers, tanks, cryostats, and transfer systems for transportation and storage of LNG, LPG, liquid nitrogen and liquid helium. The chemical composition is optimized for cryogenic applications in terms of impact strength and other characteristics. It has controlled chemical composition and ferrite content for resistance to microfissuring, and balanced minor additions of certain elements for optimum arc stability and wetting characteristics. Impurity levels are lower in the consumable in order to reduce the risk of hot cracking and to obtain the best arc stability, fluidity, low spatter and wetting properties.

BUY NOW


Recommended Welding Parameters

Current Voltage Wire Diameter Wire Feed Speed
60-220 A 15-28 V 1.0 mm (0.040 in.) 4.0-12.0 m/min (157-472 in./min)
150-260 A 24-29 V 1.2 mm (0.047 in.) 3.0-10.0 m/min (118-394 in./min)

Classifications

Wire Electrode Werkstoffnummer : ~1.4430
SFA/AWS A5.9 : ER316L
EN ISO 14343-A : G (19 12 3 L)

Approvals

Grade EN 13479
Society CE
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Austenitic (with appr. 2 % ferrite) 19 % Cr - 13 % Ni - 2 % Mo - Low C
Shielding Gas I1, M12, M13 (EN ISO 14175)

Typical Weld Metal Analysis %

Typical Wire Composition %
Al C Co Cr Cu FN WRC-92 Mn Mo N Nb Ni P S Si Ti
0.01 % 0.02 % 0.03 % 18.5 % 0.06 % 2 % 1.8 % 2.3 % 0.06 % 0.01 % 13.3 % 0.012 % 0.003 % 0.4 % 0.005 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton 316L Cryo
SF30109820 FIND A DISTRIBUTOR
SF30129820 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..