Exaton 16.5.1
16.5.1 is a filler material for joining EN 1.4418 and similar steels. It is also used for overlay welding. The weld metal has excellent resistance to cavitation and is used typically for shafts, propellers, pumps and valves in for example, hydropower generation. It is used for MIG/MAG welding.

Documents
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
C | Cr | Mn | Mo | Ni | P | S | Si | |||||||
<=0.020 % | 16 % | 1.4 % | 1 % | 5.5 % | <=0.025 % | <=0.015 % | 0.4 % |
Typical Charpy V-Notch Properties
Testing Temperature | 20 degC |
Impact Value (met) | 80 J |
PWHT |
Classifications
Name | EN ISO 14343-A |
Grade | G 16 5 1 |
2 |
Typical Tensile Properties
Condition | Elongation |
PWHT | 22 % |
Deposition Data
Wire Feed Speed | 3.0-3.0 m/min |
Wire Feed Speed | 118-118 in./min |
Voltage | 24-29 V |
Diameter | 1.2 mm |
Diameter | 0.047 in. |
Deposition Rate | 0.0-0.0 kg/h |
Deposition Rate | 0.0-0.0 lb/h |
Current | 150-260 A |