2594 is a high alloyed chromium-nickel-molybdenum-nitrogen covered electrode with basic coating for welding of 25%Cr- and superduplex stainless steels. The basic type of electrode combines good welding properties in all positions with high impact strength at low temperatures. The weld metal is characterized by high strength and very good corrosion resistance. Examples are: excellent stress corrosion cracking resistance, excellent pitting resistance in chloride-containing media, high resistance to general corrosion, high resistance to erosion corrosion and corrosion fatigue. 2594 is used for welding of super duplex stainless steels in service temperatures up to 280°C (536°F), where good impact strength at temperatures down to -50°C is required. Common steel types include: ISO 1.4410, 1.4501 and 1.4507; UNS: S32750, S32760, S31260 and S32550. It can also be used as overmatching consumable for 21-23%Cr duplex stainless steels.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded iso
45 J (33 ft-lb) -50 degC (-58 degF)
85 J (63 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

ConditionElongationShielding GasTensile Strength Yield Strength
As Welded26 %ISO915 MPa (133 ksi)750 MPa (109 ksi)

Deposition Data

Current Fusion time per electrode at 90% I max Deposition Rate @ 90% I max Diameter Deposition Efficiency (%) Number of electrodes/kg weld metal Voltage
50-80 A 50.2 sec 0.72 kg/h (1,6 lb/h) 2.5 x 300.0 mm (0.098 x 11,8 in.) 62 % 100 22 V
70-100 A 58.67 sec 1.2 kg/h (2,6 lb/h) 3.2 x 350.0 mm (1/8 x 13,8 in.) 65 % 53 23 V
100-150 A 2.0 kg/h (4,4 lb/h) 4.0 x 350.0 mm (5/32 x 13,8 in.) 73 % 26

Classifications

Classifications Werkstoffnummer : (1.4410)
SFA/AWS A5.4 : E2594-15
EN ISO 3581-A : E 25 9 4 N L B

Approvals

Grade EN 13479
Society CE
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Austenitic-Ferritic CrNiMo
Coating Type Basic
Ferrite Content FN 35-55
Welding Current DC+
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton 2594
68932520L0 FIND A DISTRIBUTOR
68933230T0 FIND A DISTRIBUTOR
68934030G0 FIND A DISTRIBUTOR
68932520U0 FIND A DISTRIBUTOR
68933230U0 FIND A DISTRIBUTOR
68934030U0 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..