347-17 is a niobium-stabilized chromium-nickel covered electrode with rutile coating for welding of steels of ASTM 321 and 347 types as well as overalloys. It is used in structural applications at max 400°C (752°F). When a weld metal similar to the parent metal is not required, 347-17 can be used for welding ferritic and martensitic steels. The electrode has excellent arc stability, low spatter and fast burn off rate with minimum stub loss. It is also characterised by improved moisture resistance, good slagdetachability, high resistance to porosity and easy post weld finishing. 347-17 gives smooth uniform beads and works in any standard weld position.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded iso
50 J (37 ft-lb) -20 degC (-4 degF)
35 J (26 ft-lb) -60 degC (-76 degF)
55 J (41 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

ConditionElongationShielding GasTensile Strength Yield Strength
As Welded35 %ISO620 MPa (90 ksi)490 MPa (71 ksi)

Deposition Data

Current Fusion time per electrode at 90% I max Deposition Rate @ 90% I max Diameter Deposition Efficiency (%) Number of electrodes/kg weld metal Voltage
50-90 A 38 sec 1.0 kg/h (2,2 lb/h) 2.5 x 300.0 mm (0.098 x 11,8 in.) 56 % 97 26 V
70-130 A 53 sec 1.4 kg/h (3,1 lb/h) 3.2 x 350.0 mm (1/8 x 13,8 in.) 56 % 50 28 V
90-180 A 55 sec 2.0 kg/h (4,4 lb/h) 4.0 x 350.0 mm (5/32 x 13,8 in.) 56 % 33 30 V
140-250 A 60 sec 2.9 kg/h (6,4 lb/h) 5.0 x 350.0 mm (0.197 x 13,8 in.) 56 % 21 31 V

Classifications

Classifications Werkstoffnummer : 1.4551
EN ISO 3581-A : E 19 9 Nb R 1 2
SFA/AWS A5.4 : E347-17

Approvals

Society CE
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Austenitic CrNi
Coating Type Acid Rutile
Ferrite Content FN 6-9
Welding Current DC+, AC

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu FN WRC-92 Mn Mo Nb Nb+Ta Ni P S Si
0.03 % 20 % 0.07 % 7 % 0.8 % 0.07 % 0.29 % 0.29 % 10 % 0.019 % 0.010 % 0.7 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton 347-17
69004040U0 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..