316/316L-17 is a chromium-nickel-molybdenum covered electrode with rutile coating for welding of low carbon, molybdenum alloyed, austenitic stainless steels of 316L (1.4436) type. 316/316L-17 is used for welding steel of the types ISO: 1,4401, 1,4404, 1,4435, 1.4436, 1.4571 and ASTM: 316, 316L, 316LN, 316H and 316Ti. In cases where creep strength is of secondary importance, 316/316L-17 is suitable for welding of corresponding stabilized austenitic steels. When a weld metal similar to the parent metal is not required, 316/316L-17 can be used for welding ferritic and martensitic steels.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded iso
36 J (27 ft-lb) -105 degC (-157 degF)
60 J (44 ft-lb) -20 degC (-4 degF)
70 J (52 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

ConditionElongationShielding GasTensile Strength Yield Strength
As Welded35 %ISO590 MPa (86 ksi)470 MPa (68 ksi)

Deposition Data

Current Fusion time per electrode at 90% I max Deposition Rate @ 90% I max Diameter Deposition Efficiency (%) Number of electrodes/kg weld metal Voltage
45-90 A 45 sec 0.9 kg/h (2,0 lb/h) 2.5 x 300.0 mm (0.098 x 11,8 in.) 55 % 96 29 V
60-125 A 57 sec 1.4 kg/h (3,1 lb/h) 3.2 x 350.0 mm (1/8 x 13,8 in.) 55 % 52 30 V
70-190 A 57 sec 2.0 kg/h (4,4 lb/h) 4.0 x 350.0 mm (5/32 x 13,8 in.) 56 % 34 32 V
100-280 A 63 sec 3.0 kg/h (6,6 lb/h) 5.0 x 350.0 mm (0.197 x 13,8 in.) 56 % 21 32 V

Classifications

Classifications EN ISO 3581-A : E 19 12 3 L R 1 2
SFA/AWS A5.4 : E316L-17
Werkstoffnummer : 1.4430
CSA W48 : E316L-17

Approvals

Approvals CE EN 13479
CWB CSA W48: E316L-17
VdTÜV 07789
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Austenitic CrNiMo
Coating Type Acid Rutile
Ferrite Content FN 3-10
Welding Current DC+, AC

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr FN WRC-92 Mn Mo N Ni Si
0.02 % 18.5 % 3 % 0.8 % 2.8 % 0.10 % 12 % 1 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Exaton 316/316L-17
68952520L0 FIND A DISTRIBUTOR
68953230T0 FIND A DISTRIBUTOR
68954030G0 FIND A DISTRIBUTOR
68955030G0 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..